We study anomalous scaling and multi-scaling of two-dimensional crack profiles in the random fuse model using both periodic and open boundary conditions. Our large scale and extensively sampled numerical results reveal the importance of crack branching and coalescence of microcracks, which induce jumps in the solid-on-solid crack profiles. Removal of overhangs (jumps) in the crack profiles eliminates the multiscaling observed in earlier studies and reduces anomalous scaling. We find that the probability density distribution p(Delta h(l)) of the height differences Delta h(l) = [h(x+l)-h(x)] of the crack profile obtained after removing the jumps in the profiles has the scaling form p(Delta h(l)) = (Delta h(2)(l)>(-1/2) f(Delta h(l)/(Delta h(2)(l)>(1/2)), and follows a Gaussian distribution even for small bin sizes l. The anomalous scaling can be summarized with the scaling relation [<Delta h(2)(l)>(1/2)/(Delta h(2)(L/2)>(1/2)](1/zeta loc)+(l-L/2)(2)/(L/2)(2) = 1, where <Delta h(2)(L/2)>(1/2) similar to L-zeta and L is the system size.

Anomalous roughness of fracture surfaces in 2D fuse models

Zapperi S;
2008

Abstract

We study anomalous scaling and multi-scaling of two-dimensional crack profiles in the random fuse model using both periodic and open boundary conditions. Our large scale and extensively sampled numerical results reveal the importance of crack branching and coalescence of microcracks, which induce jumps in the solid-on-solid crack profiles. Removal of overhangs (jumps) in the crack profiles eliminates the multiscaling observed in earlier studies and reduces anomalous scaling. We find that the probability density distribution p(Delta h(l)) of the height differences Delta h(l) = [h(x+l)-h(x)] of the crack profile obtained after removing the jumps in the profiles has the scaling form p(Delta h(l)) = (Delta h(2)(l)>(-1/2) f(Delta h(l)/(Delta h(2)(l)>(1/2)), and follows a Gaussian distribution even for small bin sizes l. The anomalous scaling can be summarized with the scaling relation [(1/2)/(Delta h(2)(L/2)>(1/2)](1/zeta loc)+(l-L/2)(2)/(L/2)(2) = 1, where (1/2) similar to L-zeta and L is the system size.
2008
INFM
CRACK-PROPAGATION
BRITTLE-FRACTURE
INTERFACES
MORPHOLOGY
WOOD
File in questo prodotto:
Non ci sono file associati a questo prodotto.

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/20.500.14243/119953
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus ND
  • ???jsp.display-item.citation.isi??? ND
social impact