Er3+/Yb3+-codoped 94SiO2-6TiO2 planar waveguides, with 1 mol% Er and molar ratio Yb/Er =2, were fabricated by rf-sputtering technique. All waveguides were single-mode at 1550 nm. An attenuation coefficient of 0.5 dB/cm at 632.8 nm and a lifetime of the 4I13/2 metastabile state of 7.2 ms were measured. Upon cw excitation at 978 nm, an increase of the 1.53 ?m luminescence intensity larger than two-fold was detected in the Yb3+/Er3+-codoped waveguide with respect to the waveguide doped only with Er3+.

Enhanced spectroscopic properties at 1.5 um in Er3+/Yb 3+-activated silica-titania planar waveguides fabricated by rf-sputtering

A Chiasera;S Pelli;M Ferrari;
2003

Abstract

Er3+/Yb3+-codoped 94SiO2-6TiO2 planar waveguides, with 1 mol% Er and molar ratio Yb/Er =2, were fabricated by rf-sputtering technique. All waveguides were single-mode at 1550 nm. An attenuation coefficient of 0.5 dB/cm at 632.8 nm and a lifetime of the 4I13/2 metastabile state of 7.2 ms were measured. Upon cw excitation at 978 nm, an increase of the 1.53 ?m luminescence intensity larger than two-fold was detected in the Yb3+/Er3+-codoped waveguide with respect to the waveguide doped only with Er3+.
2003
Istituto di Fisica Applicata - IFAC
Istituto di fotonica e nanotecnologie - IFN
File in questo prodotto:
Non ci sono file associati a questo prodotto.

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/20.500.14243/121881
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus 0
  • ???jsp.display-item.citation.isi??? ND
social impact