This article points to the importance of penetrating micropores through the graft wall to minimize thrombosis and to enhance endothelialization in small diameter polymer skin coated vascular grafts. Four types of spongy polyurethane-polydimethylsiloxane vascular grafts (PUG) fabricated by a spray, phase-inversion technique, 1.5 mm inner diameter, 1.5-1.9 cm in length, were implanted end-to-end in the infrarenal aorta of 26 adult rats. Some had a continuous inner skin and a hydraulic permeability (HP) of 0 ml/min/cm(2)/120 mmHg (PUG-S-0). Some had an inner skin with varying amounts of isolated penetrating micropores and a mean hydraulic permeability of 11 (PUG-S-11), 37 (PUC-S-37), or 58 ml/min/cm(2)/120 mmHg (PUG-S-58). Twelve PUC-S-0, 6 PUG-S-11, 4 PUG-S-11, and 4 PUG-S-58 were evaluated between 2 hr and 3 months after implantation. All PUC-S-0 occluded soon after implantation. The PUG that had a HP of more than 11 ml/min/cm(2) showed acceptable patency. However, endothelialization was limited to anastomoses in patent PUG-S-11. In contrast, the patent PUG-S-37 and PUG-S-58 were largely endothelialized. In all patent grafts at 3 months, numerous host cells had migrated, and newly formed capillaries were seen in the voids of the graft wall, which appeared moderately to highly cellular. In conclusion, it appears that penetrating micropores through the graft wall increase patency and that a highly porous structure is needed to achieve extensive endothelialization in small diameter polymer skin coated vascular grafts.

Penetrating micropores increase patency and achieve extensive endothelialization in small-diameter polymer skin coated vascular grafts

SOLDANI GIORGIO;
1996

Abstract

This article points to the importance of penetrating micropores through the graft wall to minimize thrombosis and to enhance endothelialization in small diameter polymer skin coated vascular grafts. Four types of spongy polyurethane-polydimethylsiloxane vascular grafts (PUG) fabricated by a spray, phase-inversion technique, 1.5 mm inner diameter, 1.5-1.9 cm in length, were implanted end-to-end in the infrarenal aorta of 26 adult rats. Some had a continuous inner skin and a hydraulic permeability (HP) of 0 ml/min/cm(2)/120 mmHg (PUG-S-0). Some had an inner skin with varying amounts of isolated penetrating micropores and a mean hydraulic permeability of 11 (PUG-S-11), 37 (PUC-S-37), or 58 ml/min/cm(2)/120 mmHg (PUG-S-58). Twelve PUC-S-0, 6 PUG-S-11, 4 PUG-S-11, and 4 PUG-S-58 were evaluated between 2 hr and 3 months after implantation. All PUC-S-0 occluded soon after implantation. The PUG that had a HP of more than 11 ml/min/cm(2) showed acceptable patency. However, endothelialization was limited to anastomoses in patent PUG-S-11. In contrast, the patent PUG-S-37 and PUG-S-58 were largely endothelialized. In all patent grafts at 3 months, numerous host cells had migrated, and newly formed capillaries were seen in the voids of the graft wall, which appeared moderately to highly cellular. In conclusion, it appears that penetrating micropores through the graft wall increase patency and that a highly porous structure is needed to achieve extensive endothelialization in small diameter polymer skin coated vascular grafts.
1996
Istituto di Fisiologia Clinica - IFC
File in questo prodotto:
File Dimensione Formato  
prod_227168-doc_55722.pdf

accesso aperto

Descrizione: Penetrating micropores increase patency and achieve extensive endothelialization in small-diameter polymer skin coated vascular grafts
Dimensione 381.97 kB
Formato Adobe PDF
381.97 kB Adobe PDF Visualizza/Apri

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/20.500.14243/124549
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus ND
  • ???jsp.display-item.citation.isi??? 16
social impact