Aging and memory are phenomena that can be found in various disordered systems. Memory of multiple aging stages has been found in spin glasses, below the so called freezing temperature Tf and in the relaxor ferroelectric PLZT also above this temperature, but it is not sure whether memory at these temperature is intrinsic of the glassy relaxor system or is rather due to migration of mobile defects. We measured anelastic and dielectric susceptibility in two different PLZT compositions: relaxor (PLZT 9/65/35) and partially ferroelectric (PLZTN 7/60/40) with 0.02 oxygen vacancies. We introduced O vacancies, H defects and mobile charges resulting from their ionization in the relaxor and we found that in this sample, memory, in elastic compliance and dielectric susceptibility, is not enhanced but depressed by an increase of O vacancies, while in the ferroelectric, there is no memory unless aging is protracted for long times. This is considered as evidence that in the relaxor case memory is intrinsic while in the non relaxor case it is due to slow migration of defects.

Aging, Memory and Oxygen Vacancies in PLZT

Cordero F;Craciun F;Galassi C
2007

Abstract

Aging and memory are phenomena that can be found in various disordered systems. Memory of multiple aging stages has been found in spin glasses, below the so called freezing temperature Tf and in the relaxor ferroelectric PLZT also above this temperature, but it is not sure whether memory at these temperature is intrinsic of the glassy relaxor system or is rather due to migration of mobile defects. We measured anelastic and dielectric susceptibility in two different PLZT compositions: relaxor (PLZT 9/65/35) and partially ferroelectric (PLZTN 7/60/40) with 0.02 oxygen vacancies. We introduced O vacancies, H defects and mobile charges resulting from their ionization in the relaxor and we found that in this sample, memory, in elastic compliance and dielectric susceptibility, is not enhanced but depressed by an increase of O vacancies, while in the ferroelectric, there is no memory unless aging is protracted for long times. This is considered as evidence that in the relaxor case memory is intrinsic while in the non relaxor case it is due to slow migration of defects.
2007
Istituto di Scienza, Tecnologia e Sostenibilità per lo Sviluppo dei Materiali Ceramici - ISSMC (ex ISTEC)
Istituto dei Sistemi Complessi - ISC
PLZT
Oxygen vacancies
Dielectric spectroscopy
Anelastic spectroscopy
File in questo prodotto:
Non ci sono file associati a questo prodotto.

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/20.500.14243/155468
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus 5
  • ???jsp.display-item.citation.isi??? ND
social impact