In order to use MgB(2) conductors for AC applications, research and development efforts have to be carried out on their architecture and sheath material to minimize the AC losses. This paper will present the fabrication and characterization of two types of ex situ powder-in-tube processed pure MgB(2) conductors with properties making them good candidates for AC industrial applications: a multifilamentary tape with 12 filaments with a twisting pitch down to 17 mm and a 361-filament wire with an average single-filament size of about 30 mu m. Concerning the twisted tapes we will present values of critical current density of about 10(5) A cm(-2) at 4.2 K and 2 T and we will show that it is possible to achieve a proper compromise between the tape size, the twisting pitch length and the critical current density to face a reduction of the critical current density as a consequence of the strain on the filaments. Concerning the 361-multifilamentary wire we will show appreciable values of critical current density of about 5 x 10(4) A cm(-2) at 4.2 K and 2.5 T which, together with the advantages given by the high number of very thin filaments and the non-magnetic matrix, could justify their employment.

Fabrication and superconducting properties of multifilamentary MgB(2) conductors for AC purposes: twisted tapes and wires with very thin filaments

Malagoli A;Bernini C;Braccini V;Fanciulli C;Vignolo M
2009

Abstract

In order to use MgB(2) conductors for AC applications, research and development efforts have to be carried out on their architecture and sheath material to minimize the AC losses. This paper will present the fabrication and characterization of two types of ex situ powder-in-tube processed pure MgB(2) conductors with properties making them good candidates for AC industrial applications: a multifilamentary tape with 12 filaments with a twisting pitch down to 17 mm and a 361-filament wire with an average single-filament size of about 30 mu m. Concerning the twisted tapes we will present values of critical current density of about 10(5) A cm(-2) at 4.2 K and 2 T and we will show that it is possible to achieve a proper compromise between the tape size, the twisting pitch length and the critical current density to face a reduction of the critical current density as a consequence of the strain on the filaments. Concerning the 361-multifilamentary wire we will show appreciable values of critical current density of about 5 x 10(4) A cm(-2) at 4.2 K and 2.5 T which, together with the advantages given by the high number of very thin filaments and the non-magnetic matrix, could justify their employment.
2009
Istituto Superconduttori, materiali innovativi e dispositivi - SPIN
Critical currents
Superconducting wires and tapes
File in questo prodotto:
File Dimensione Formato  
prod_178222-doc_11884.pdf

non disponibili

Descrizione: articolo pubblicato
Dimensione 1.23 MB
Formato Adobe PDF
1.23 MB Adobe PDF   Visualizza/Apri   Richiedi una copia

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/20.500.14243/167950
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus ND
  • ???jsp.display-item.citation.isi??? ND
social impact