The paper reports the results of an extensive characterization of the Ti6Al4V-SiCf composite produced by hot isostatic pressing (HIP) to assess its capability to withstand the inservice conditions of turbine blades operating at middle temperatures in aeronautical engines. The microstructure of composite, in as-fabricated condition and after long-term heat treatments (up to 1,000 hours) in the temperature range 673-873 K, has been investigated by means of different techniques. Particular attention was paid to the micro-chemical evolution of fibre-matrix interface which is scarcely affected also by the most severe heat treatments examined here. This leads to stable mechanical properties as evidenced by hardness, tensile and FIMEC instrumented indentation tests. Therefore, the composite can operate at the maximum temperature (873 K) foreseen for its aeronautical applications without remarkable modifications of its microstructure and degradation of mechanical properties. The mechanical characterization has been completed by internal friction and dynamic modulus measurements carried out both at constant and increasing temperature, from 80 to 1173 K.

Micro-chemistry and mechanical behaviour of Ti6A14V-SiCf composite produced by HIP for aeronautical applications

R Donnini;S Kaciulis;A Mezzi;
2011

Abstract

The paper reports the results of an extensive characterization of the Ti6Al4V-SiCf composite produced by hot isostatic pressing (HIP) to assess its capability to withstand the inservice conditions of turbine blades operating at middle temperatures in aeronautical engines. The microstructure of composite, in as-fabricated condition and after long-term heat treatments (up to 1,000 hours) in the temperature range 673-873 K, has been investigated by means of different techniques. Particular attention was paid to the micro-chemical evolution of fibre-matrix interface which is scarcely affected also by the most severe heat treatments examined here. This leads to stable mechanical properties as evidenced by hardness, tensile and FIMEC instrumented indentation tests. Therefore, the composite can operate at the maximum temperature (873 K) foreseen for its aeronautical applications without remarkable modifications of its microstructure and degradation of mechanical properties. The mechanical characterization has been completed by internal friction and dynamic modulus measurements carried out both at constant and increasing temperature, from 80 to 1173 K.
2011
Istituto per lo Studio dei Materiali Nanostrutturati - ISMN
Anelastic behaviour; Matrix-fibre interface; Mechanical properties; Microstructural stability; Ti6Al4V-SiCf composite
File in questo prodotto:
File Dimensione Formato  
prod_169894-doc_90368.pdf

solo utenti autorizzati

Descrizione: Micro-chemistry and mechanical behaviour of Ti6A14V-SiCf composite produced by HIP for aeronautical applications
Dimensione 1.87 MB
Formato Adobe PDF
1.87 MB Adobe PDF   Visualizza/Apri   Richiedi una copia

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/20.500.14243/169589
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus ND
  • ???jsp.display-item.citation.isi??? ND
social impact