The conventional powder-in-tube technique does not allow to produce textured Tl(1223) tapes. An electrophoretic deposition technique was used to produce uniform layers of controlled thickness on Ag substrates by a simple and reproducible procedure. A high degree of texture, comparable with the one generally observed for Bi-based tapes was obtained thanks to the appropriate grain morphology, by simply alternating deposition and uniaxial pressing. After annealing, critical current densities of 11'000 A/cm(2) were reached.

Textured Tl(1223)/Ag tapes prepared by electrophoretic deposition

Bellingeri E;
1998

Abstract

The conventional powder-in-tube technique does not allow to produce textured Tl(1223) tapes. An electrophoretic deposition technique was used to produce uniform layers of controlled thickness on Ag substrates by a simple and reproducible procedure. A high degree of texture, comparable with the one generally observed for Bi-based tapes was obtained thanks to the appropriate grain morphology, by simply alternating deposition and uniaxial pressing. After annealing, critical current densities of 11'000 A/cm(2) were reached.
1998
Inglese
11
1
77
78
Tl(1223)
texture
tapes
electrophoresis
critical current
International Workshop on Thallium and Mercury Based Superconducting Materials, CAMBRIDGE, ENGLAND, MAY 25-29, 1997
5
info:eu-repo/semantics/article
262
Bellingeri, E; Gladyshevskii, ; Re, ; Flukiger, ; R,
01 Contributo su Rivista::01.01 Articolo in rivista
none
File in questo prodotto:
Non ci sono file associati a questo prodotto.

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/20.500.14243/206441
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus ND
  • ???jsp.display-item.citation.isi??? 2
social impact