Single-phased coatings of Cr-3(C0.8N0.2)(2) have been deposited by combining a metal-organic chemical vapor deposition (MOCVD) process and an annealing post-treatment. The films were grown in the temperature range 683-793 K by low pressure MOCVD using Cr(NEt2)(4) as the single-source precursor. As-deposited films are very smooth and X-ray amorphous. A relatively low amount of nitrogen is uniformly incorporated into the film. The nitrogen content is nearly independent of the growth conditions and it amounts to exactly the value required to form the title ternary phase (similar to7 at.%). The as-deposited films crystallize upon annealing at 873 K under vacuum to form the orthorhombic Cr3(C0.8N0.2)2 phase. No evidence for additional phases has been found. Both as-deposited and annealed coatings exhibit a high hardness and a good adhesion on stainless steel substrates. The hardness increases slightly upon crystallization to typically reach 17 GPa. Preliminary properties of this metastable carbonitride phase are reported and its potential as a hard metallurgical coating is discussed.

Single-phased hard coatings of the metastable Cr3(C0.8N0.2)2 ternary phase grown by low pressure MOCVD

Ossola F;
2000

Abstract

Single-phased coatings of Cr-3(C0.8N0.2)(2) have been deposited by combining a metal-organic chemical vapor deposition (MOCVD) process and an annealing post-treatment. The films were grown in the temperature range 683-793 K by low pressure MOCVD using Cr(NEt2)(4) as the single-source precursor. As-deposited films are very smooth and X-ray amorphous. A relatively low amount of nitrogen is uniformly incorporated into the film. The nitrogen content is nearly independent of the growth conditions and it amounts to exactly the value required to form the title ternary phase (similar to7 at.%). The as-deposited films crystallize upon annealing at 873 K under vacuum to form the orthorhombic Cr3(C0.8N0.2)2 phase. No evidence for additional phases has been found. Both as-deposited and annealed coatings exhibit a high hardness and a good adhesion on stainless steel substrates. The hardness increases slightly upon crystallization to typically reach 17 GPa. Preliminary properties of this metastable carbonitride phase are reported and its potential as a hard metallurgical coating is discussed.
2000
CHIMICA INORGANICA E DELLE SUPERFICI
Istituto di Chimica della Materia Condensata e di Tecnologie per l'Energia - ICMATE
chromium carbonitride
metal-organic chemical vapor deposition
(MOCVD)
hard coating
metastable phase Cr-3(C0.8N0.2)(2)
File in questo prodotto:
File Dimensione Formato  
prod_216040-doc_50160.pdf

solo utenti autorizzati

Descrizione: Single-phased hard coatings of the metastable Cr3(C0.8N0.2)2 ternary phase grown by low pressure MOCVD
Dimensione 990.97 kB
Formato Adobe PDF
990.97 kB Adobe PDF   Visualizza/Apri   Richiedi una copia

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/20.500.14243/217282
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus ND
  • ???jsp.display-item.citation.isi??? 7
social impact