In the present work we report an anelastic spectroscopy study of pure FeCO3 (siderite) and of carbon steel samples covered by siderite films. Uncovered steel samples have also been investigated for reference. The siderite shows two relaxation processes below room temperature, at about 220 K and 140 K, while the covered steel sample displays only the peak at lower temperature. The presence of such a relaxation can be used to monitor the deposition of siderite
Anelastic spectroscopy study of iron carbonate scales from CO2 corrosion of steel
Palumbo, O;Paolone, A;
2009
Abstract
In the present work we report an anelastic spectroscopy study of pure FeCO3 (siderite) and of carbon steel samples covered by siderite films. Uncovered steel samples have also been investigated for reference. The siderite shows two relaxation processes below room temperature, at about 220 K and 140 K, while the covered steel sample displays only the peak at lower temperature. The presence of such a relaxation can be used to monitor the deposition of sideriteFile in questo prodotto:
| File | Dimensione | Formato | |
|---|---|---|---|
|
prod_267761-doc_74302.pdf
solo utenti autorizzati
Descrizione: Anelastic spectroscopy study of iron carbonate scales from CO2 corrosion of steel
Tipologia:
Versione Editoriale (PDF)
Licenza:
NON PUBBLICO - Accesso privato/ristretto
Dimensione
433.46 kB
Formato
Adobe PDF
|
433.46 kB | Adobe PDF | Visualizza/Apri Richiedi una copia |
I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.