A high-temperature test rig to simultaneously measure electrical conductivity and thermopower is described. The apparatus allows to perform measurements in a controlled atmosphere or vacuum to protect oxygen-sensitive materials. A spring-loaded mounting placed in the cold zone reduces the thermal contact resistance between the sample and two metallic blocks (the hot side and the heat sink) even at high temperatures. The hot-side metal block is periodically heated to obtain the thermopower from the slope of DV versus DT. Conductivity is measured before each thermopower measurement by a linear four-wire method. The automatic data acquisition and analysis are controlled by a LabView-based interface. Two interchangeable setups are possible. The first one uses silver blocks and K-type thermocouples and is suitable for temperatures from 300 K to about 1000 K. The second one uses W blocks and S-type thermocouples to allow higher-temperature measurements since all the hot-zone parts are made of Al2O3, Pt or W. The device was tested using PdAg alloy and Ni rods and, for the low-temperature range, the NIST standard reference material 3451 (bismuth telluride), strictly confirming the reference data.

Test rig for high temperature thermopower and electrical conductivity measurements

Boldrini S;Famengo A;Montagner F;Battiston S;Fiameni S;Fabrizio M;Barison S
2013

Abstract

A high-temperature test rig to simultaneously measure electrical conductivity and thermopower is described. The apparatus allows to perform measurements in a controlled atmosphere or vacuum to protect oxygen-sensitive materials. A spring-loaded mounting placed in the cold zone reduces the thermal contact resistance between the sample and two metallic blocks (the hot side and the heat sink) even at high temperatures. The hot-side metal block is periodically heated to obtain the thermopower from the slope of DV versus DT. Conductivity is measured before each thermopower measurement by a linear four-wire method. The automatic data acquisition and analysis are controlled by a LabView-based interface. Two interchangeable setups are possible. The first one uses silver blocks and K-type thermocouples and is suitable for temperatures from 300 K to about 1000 K. The second one uses W blocks and S-type thermocouples to allow higher-temperature measurements since all the hot-zone parts are made of Al2O3, Pt or W. The device was tested using PdAg alloy and Ni rods and, for the low-temperature range, the NIST standard reference material 3451 (bismuth telluride), strictly confirming the reference data.
2013
Istituto di Chimica della Materia Condensata e di Tecnologie per l'Energia - ICMATE
Thermoelectricity
electrical measurements
high-temperature testing
File in questo prodotto:
Non ci sono file associati a questo prodotto.

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/20.500.14243/221298
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus 19
  • ???jsp.display-item.citation.isi??? ND
social impact