Infrared spectroscopy (FTIR) is a commonly available tool in laboratories dealing with both degradation of materials and conservation of art objects to evaluate their condition. In this paper FTIR was engaged to study degradation of fibroin included in silk samples (Bombyx mori) artificially aged at various conditions (oxygen, water vapor and volatile organic products) at temperature of 150 degrees C. The results collected by Attenuated Total Reflectance/Fourier Transform Infrared Spectroscopy (ATR/FTIR) were validated by UV/Vis, XRD and SEC analyses. Based on the results, the degradation estimators were verified and classified as: (1) crystallinity defined as ratio of absorbance at 1620 and at 1656 cm(-1), A(1620)/A(1656) [1], or at 1620 and 1699 cm(-1), A(1620)/A(1699) [2]; or ratio of areas under fitted curves of band at 1261 and 1230 cm(-1), P-1261/P-1230 [3], (2) oxidation - A(1620)/A(1514) and (3) depolymerization - P-1318/P-1442. Degradation gauges defined in such a way indicate that upon artificial aging water vapor and oxygen has the most profound impact on the progress of silk degradation. It also indicates that oxygen-lean conditions stabilize silk at elevated temperature. (C) 2014 Elsevier Ltd. All rights reserved.

Degradation markers of fibroin in silk through infrared spectroscopy

M. Missori;
2014

Abstract

Infrared spectroscopy (FTIR) is a commonly available tool in laboratories dealing with both degradation of materials and conservation of art objects to evaluate their condition. In this paper FTIR was engaged to study degradation of fibroin included in silk samples (Bombyx mori) artificially aged at various conditions (oxygen, water vapor and volatile organic products) at temperature of 150 degrees C. The results collected by Attenuated Total Reflectance/Fourier Transform Infrared Spectroscopy (ATR/FTIR) were validated by UV/Vis, XRD and SEC analyses. Based on the results, the degradation estimators were verified and classified as: (1) crystallinity defined as ratio of absorbance at 1620 and at 1656 cm(-1), A(1620)/A(1656) [1], or at 1620 and 1699 cm(-1), A(1620)/A(1699) [2]; or ratio of areas under fitted curves of band at 1261 and 1230 cm(-1), P-1261/P-1230 [3], (2) oxidation - A(1620)/A(1514) and (3) depolymerization - P-1318/P-1442. Degradation gauges defined in such a way indicate that upon artificial aging water vapor and oxygen has the most profound impact on the progress of silk degradation. It also indicates that oxygen-lean conditions stabilize silk at elevated temperature. (C) 2014 Elsevier Ltd. All rights reserved.
2014
Istituto dei Sistemi Complessi - ISC
Fibroin
ATR-FTIR spectroscopy
UV/Vis spectroscopy
XRD
SEC
Degradation estimators
File in questo prodotto:
File Dimensione Formato  
prod_288165-doc_82767.pdf

solo utenti autorizzati

Descrizione: Non-anomalous diffusion is not always Gaussian
Tipologia: Versione Editoriale (PDF)
Licenza: NON PUBBLICO - Accesso privato/ristretto
Dimensione 3.83 MB
Formato Adobe PDF
3.83 MB Adobe PDF   Visualizza/Apri   Richiedi una copia

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/20.500.14243/229195
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus 128
  • ???jsp.display-item.citation.isi??? 115
social impact