We present a study and a comparison of the laser performance achieved by using 10at.%, 15at.% at. and 20at.% Yb3+: LuAG crystals longitudinally pumped at 936 nm in quasi-continuous wave.
A comparison of the laser performance of Yb3+: LuAG crystals with different doping levels
Pirri A;Vannini M;Toci G
2014
Abstract
We present a study and a comparison of the laser performance achieved by using 10at.%, 15at.% at. and 20at.% Yb3+: LuAG crystals longitudinally pumped at 936 nm in quasi-continuous wave.File in questo prodotto: