The present work highlights the progress in the field of polymeric package reliability engineering for a flexible thermoelectric generator realized by thin-film technology on a Kapton substrate. The effects of different plasma treatments on the mechanical performance at the interface of a poly-(dimethylsiloxane) (PDMS)/Kapton assembly were investigated. To increase the package mechanical stability of the realized wearable power source, the Kapton surface wettability after plasma exposure was investigated by static contact-angle measurements using deionized water and PDMS as test liquids. In fact, the well-known weak adhesion between PDMS and Kapton can lead to a delamination of the package with an unrecoverable damage of the generator. The plasma effect on the adhesion performances was evaluated by the scratch-test method. The best result was obtained by performing a nitrogen plasma treatment at a radio-frequency power of 20 W and a gas flow of 20 sccm, with a measured critical load of 1.45 N, which is 2.6 times greater than the value measured on an untreated Kapton substrate and 1.9 times greater than the one measured using a commercial primer.

PDMS/Kapton Interface Plasma Treatment Effects on the Polymeric Package for a Wearable Thermoelectric Generator

Francioso L;De Pascali C;Siciliano P;
2013

Abstract

The present work highlights the progress in the field of polymeric package reliability engineering for a flexible thermoelectric generator realized by thin-film technology on a Kapton substrate. The effects of different plasma treatments on the mechanical performance at the interface of a poly-(dimethylsiloxane) (PDMS)/Kapton assembly were investigated. To increase the package mechanical stability of the realized wearable power source, the Kapton surface wettability after plasma exposure was investigated by static contact-angle measurements using deionized water and PDMS as test liquids. In fact, the well-known weak adhesion between PDMS and Kapton can lead to a delamination of the package with an unrecoverable damage of the generator. The plasma effect on the adhesion performances was evaluated by the scratch-test method. The best result was obtained by performing a nitrogen plasma treatment at a radio-frequency power of 20 W and a gas flow of 20 sccm, with a measured critical load of 1.45 N, which is 2.6 times greater than the value measured on an untreated Kapton substrate and 1.9 times greater than the one measured using a commercial primer.
2013
Istituto per la Microelettronica e Microsistemi - IMM
File in questo prodotto:
Non ci sono file associati a questo prodotto.

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/20.500.14243/263014
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus ND
  • ???jsp.display-item.citation.isi??? ND
social impact