An analysis concerning the bulk etch rate of different type of CR-39 subjected to a chemical etching in 5.4 N KOH solution at 80 degrees C is carried out in the present work. The response of PADC samples has been evaluated adopting the fission fragment track diameter method. A standard quality control program for etching has been set up by monitoring the electrical conductivity of the etchant. Since the properties of the etching solution are constant during the etching process the difference in the Vb values are connected to the intrinsic characteristics of the CR-39 plastic such as polymerization processes. (C) 2009 Elsevier Ltd. All rights reserved.

An extended study of the etching characteristics of CR-39 detectors

D'Alessandro M;
2009

Abstract

An analysis concerning the bulk etch rate of different type of CR-39 subjected to a chemical etching in 5.4 N KOH solution at 80 degrees C is carried out in the present work. The response of PADC samples has been evaluated adopting the fission fragment track diameter method. A standard quality control program for etching has been set up by monitoring the electrical conductivity of the etchant. Since the properties of the etching solution are constant during the etching process the difference in the Vb values are connected to the intrinsic characteristics of the CR-39 plastic such as polymerization processes. (C) 2009 Elsevier Ltd. All rights reserved.
2009
CR-39
Bulk etch rate
Fission fragment method
File in questo prodotto:
Non ci sono file associati a questo prodotto.

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/20.500.14243/283079
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus ND
  • ???jsp.display-item.citation.isi??? ND
social impact