The ability of Ce-containing biOactive glasses to inhibit,oxidative stress in terms of reduction of hydrogen peroxide, by mimicking the catalase enzyme activity is demonstrated here for the 'first time. The antioxidant properties of three bioactive glasses containing an increasing amount of CeO2 have been evaluated by following the degradation of hydrogen peroxide with time after immersion in H2O2 aqueous solutions with different concentration. XPS and UV vis measurements allowed us to determine the Ce3+/Ce4+ ratio in the bulk and on the glass surface, and to correlate it with the ability of the samples to show catalase mimetic activity. Interestingly, we have found that the bioactive glass with composition 23.2Na(2)O-25.7CaO-43.4SiO(2)-2.4P(2)O(5)-5.3Ce02 immersed in 0.1 H2O2 aqueous solutionis able to degrade 90% of it in 1 week. The reduction in bioactivity of the glasses with increasing CeO2 content is here rationalized in terms of a lower amount of phosphate groups available for the hydroxyapatite layer formation, after binding with cerium ions. In fact classical molecular dynamics simulations revealed that the addition of CeO2 leads to the formation of cerium phosphate rich regions. The formation of an insoluble CePO4 crystalline phase is also observed by XRD analysis after thermal treatment of the glass samples.
Evidence of catalase mimetic activity in Ce3+/Ce4+ doped bioactive glasses
Luches P;Valeri S
2015
Abstract
The ability of Ce-containing biOactive glasses to inhibit,oxidative stress in terms of reduction of hydrogen peroxide, by mimicking the catalase enzyme activity is demonstrated here for the 'first time. The antioxidant properties of three bioactive glasses containing an increasing amount of CeO2 have been evaluated by following the degradation of hydrogen peroxide with time after immersion in H2O2 aqueous solutions with different concentration. XPS and UV vis measurements allowed us to determine the Ce3+/Ce4+ ratio in the bulk and on the glass surface, and to correlate it with the ability of the samples to show catalase mimetic activity. Interestingly, we have found that the bioactive glass with composition 23.2Na(2)O-25.7CaO-43.4SiO(2)-2.4P(2)O(5)-5.3Ce02 immersed in 0.1 H2O2 aqueous solutionis able to degrade 90% of it in 1 week. The reduction in bioactivity of the glasses with increasing CeO2 content is here rationalized in terms of a lower amount of phosphate groups available for the hydroxyapatite layer formation, after binding with cerium ions. In fact classical molecular dynamics simulations revealed that the addition of CeO2 leads to the formation of cerium phosphate rich regions. The formation of an insoluble CePO4 crystalline phase is also observed by XRD analysis after thermal treatment of the glass samples.I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.