The "swelling-poling-deswelling" technique is a new procedure of poling crosslinked polymeric networkcarrying covalently attached NLO (nonlinear optical) chromophores. It is based upon a solvent-swollencrosslinked polymeric network before submission to poling. Under electrical poling, the matrix is deswelledwithout heating above the polymer Tg (glass transition temperature) obtaining a significant improvement ofthe stabilization of the alignment of the chromophores and therefore of the SHG (second harmonicgeneration). We determined the d33 values of DR1 chromophore linked in different manner to PMMA(polymethylmethacrylate) and polystyrene. Crosslinked PMMA gives very good results, in fact the 40% of thed33 value remains after 4 months respect to d33 evaluated a couple of hours after poling. Interestingly thesame stability in the time of the d33 is observed with the crosslinked polystyrene matrix. In terms of d33 afterpoling, the two systems carrying DR1 (Disperse Red 1) moieties covalently attached to the polystyrene matrix(side-chain and crosslinked) behave in a similar manner, but in terms of stability, the linear polymeric systemis the best (75%), higher than all systems investigated.
Evidence for the applicability of a novel procedure (swelling-poling- deswelling) to produce a stable alignment of second order NLO-chromophores covalently attached to a cross-linked PMMA or polystyrene polymeric network
Marinotto, Daniele;Pietralunga, Silvia Maria
2011
Abstract
The "swelling-poling-deswelling" technique is a new procedure of poling crosslinked polymeric networkcarrying covalently attached NLO (nonlinear optical) chromophores. It is based upon a solvent-swollencrosslinked polymeric network before submission to poling. Under electrical poling, the matrix is deswelledwithout heating above the polymer Tg (glass transition temperature) obtaining a significant improvement ofthe stabilization of the alignment of the chromophores and therefore of the SHG (second harmonicgeneration). We determined the d33 values of DR1 chromophore linked in different manner to PMMA(polymethylmethacrylate) and polystyrene. Crosslinked PMMA gives very good results, in fact the 40% of thed33 value remains after 4 months respect to d33 evaluated a couple of hours after poling. Interestingly thesame stability in the time of the d33 is observed with the crosslinked polystyrene matrix. In terms of d33 afterpoling, the two systems carrying DR1 (Disperse Red 1) moieties covalently attached to the polystyrene matrix(side-chain and crosslinked) behave in a similar manner, but in terms of stability, the linear polymeric systemis the best (75%), higher than all systems investigated.| File | Dimensione | Formato | |
|---|---|---|---|
|
prod_327994-doc_111826.pdf
solo utenti autorizzati
Descrizione: Evidence for the applicability of a novel procedure (swelling-poling- deswelling) to produce a stable alignment of second order NLO-chromophores
Tipologia:
Versione Editoriale (PDF)
Licenza:
NON PUBBLICO - Accesso privato/ristretto
Dimensione
514.26 kB
Formato
Adobe PDF
|
514.26 kB | Adobe PDF | Visualizza/Apri Richiedi una copia |
I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.