This paper concerns the recovery of zinc from fly ashes generated by incineration plant of automobile tire wastes. The recovery is obtained by two extraction steps with a pH-controlled ammonia chloride solution. The ashes contain about 51% wt of zinc, 1% wt of iron and aluminium and small quantities (less than 0.1% wt) of cobalt, copper and lead. Various factors affect the performance and efficiency of leaching: temperature, concentration, pH and time were studied using a factorial experimental design. After two steps with ammonium chloride 3mol/L, L/S=6 ml/g, pH 5.4 and T=72°C the leaching liquor has been purified in a sample step by cementation with metallic zinc powder without activation. Traces of Pb,As,Sb,Se,Mo,Ni have been cleared by cementation with zinc. The fly ash and residue composition was determined by X-ray and its elemental composition by ICP-OES and IC. The obtained results show that recovery efficiency amounts to 98% wt for zinc; the concentration of zinc in the leach liquors reaches more than 45g/L while most of the iron is not leached. The purified solution containing zinc allows the direct recovery of high grade zinc by electro-deposition.
RECOVERY OF ZINC FROM ASHES OF AUTOMOBILE TIRE WASTES BY PH CONTROLLED SOLUTIONS OF AMMONIUM CHLORIDE
PIelpo;G Chita;F Baldassarre
2008
Abstract
This paper concerns the recovery of zinc from fly ashes generated by incineration plant of automobile tire wastes. The recovery is obtained by two extraction steps with a pH-controlled ammonia chloride solution. The ashes contain about 51% wt of zinc, 1% wt of iron and aluminium and small quantities (less than 0.1% wt) of cobalt, copper and lead. Various factors affect the performance and efficiency of leaching: temperature, concentration, pH and time were studied using a factorial experimental design. After two steps with ammonium chloride 3mol/L, L/S=6 ml/g, pH 5.4 and T=72°C the leaching liquor has been purified in a sample step by cementation with metallic zinc powder without activation. Traces of Pb,As,Sb,Se,Mo,Ni have been cleared by cementation with zinc. The fly ash and residue composition was determined by X-ray and its elemental composition by ICP-OES and IC. The obtained results show that recovery efficiency amounts to 98% wt for zinc; the concentration of zinc in the leach liquors reaches more than 45g/L while most of the iron is not leached. The purified solution containing zinc allows the direct recovery of high grade zinc by electro-deposition.I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.