Hydrophobic membrane is desired to avoid pore wetting phenomenon in membrane distillation (MD). In the present paper, highly hydrophobic Hyflon AD60/PVDF composite hollow fiber membranes were prepared by coating a copolymer (Hyflon AD60) of tetrafluoroethylene (TFE) and 2,2,4-trifluoro-5-trifluoro methoxy-1,3-dioxole (TTD) on poly(vinylidene fluoride) (PVDF) membranes. The effects of Hyflon AD60 concentration, coating time, heat-treatment temperature and heat-treatment time on the structures and performances of Hyflon AD60/PVDF composite hollow fiber membranes in vacuum membrane distillation (VMD) process were investigated. The results show that the hydrophobicity of PVDF hollow fiber membrane was significantly improved by coating Hyflon AD60. The optimized Hyflon AD60 concentration, coating time, heat-treatment temperature and heat-treatment time were 0.1 wt%, 10-20 min, 40-50 C and 9 h, respectively. Employing NaCl solution with concentration of 35 g L1, under a vacuum of 0.09 MPa and feed temperature of 70 C, the water flux and salt rejection of the composite hollow fiber membrane in VMD process reached to approximately 10 kg m2 h1 and higher than 99.9 %, respectively, and kept stable, indicating that Hyflon AD60/PVDF composite membrane is an excellent candidate for operation in VMD operation.

Preparation of Hyflon AD60/PVDF composite hollow fiber membranes for vacuum membrane distillation

Drioli E;
2016

Abstract

Hydrophobic membrane is desired to avoid pore wetting phenomenon in membrane distillation (MD). In the present paper, highly hydrophobic Hyflon AD60/PVDF composite hollow fiber membranes were prepared by coating a copolymer (Hyflon AD60) of tetrafluoroethylene (TFE) and 2,2,4-trifluoro-5-trifluoro methoxy-1,3-dioxole (TTD) on poly(vinylidene fluoride) (PVDF) membranes. The effects of Hyflon AD60 concentration, coating time, heat-treatment temperature and heat-treatment time on the structures and performances of Hyflon AD60/PVDF composite hollow fiber membranes in vacuum membrane distillation (VMD) process were investigated. The results show that the hydrophobicity of PVDF hollow fiber membrane was significantly improved by coating Hyflon AD60. The optimized Hyflon AD60 concentration, coating time, heat-treatment temperature and heat-treatment time were 0.1 wt%, 10-20 min, 40-50 C and 9 h, respectively. Employing NaCl solution with concentration of 35 g L1, under a vacuum of 0.09 MPa and feed temperature of 70 C, the water flux and salt rejection of the composite hollow fiber membrane in VMD process reached to approximately 10 kg m2 h1 and higher than 99.9 %, respectively, and kept stable, indicating that Hyflon AD60/PVDF composite membrane is an excellent candidate for operation in VMD operation.
2016
Istituto per la Tecnologia delle Membrane - ITM
Composite hollow fiber membrane
Hydrophobic modification
Hyflon AD60
Poly(vinylidene fluoride)
Vacuum membrane distillation
File in questo prodotto:
File Dimensione Formato  
prod_353642-doc_114408.pdf

non disponibili

Descrizione: Preparation of Hyflon AD60/PVDF composite hollow fiber membranes for vacuum membrane distillation
Tipologia: Versione Editoriale (PDF)
Dimensione 1.31 MB
Formato Adobe PDF
1.31 MB Adobe PDF   Visualizza/Apri   Richiedi una copia

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/20.500.14243/311881
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus 77
  • ???jsp.display-item.citation.isi??? ND
social impact