Geopolymer monoliths with controlled lamellar macroporosity and total porosity ranging from 60% to 70% were prepared by ice-templating a partially geopolymerized slurry. Both the maturation treatment of the starting mixture and the water specifically added for freeze-casting were tailored to modify both the geopolymerization and viscosity of the slurry, and, consequently, its freezing behavior, in order to optimize the final lamellar architecture. Following a room temperature maturation treatment, a 50% water content added for freezing developed thick lamellae and wide pores. A lower water content (30%) and curing at 80 °C after maturation at room temperature (for both 50% and 30% H2O) was conducive to a narrow lamellar pore width distribution in the 30-130 ?m range. However, the consumption of water due to geopolymerization in samples cured at 80 °C led to a decreased length and thickness of the lamellae. Lastly, the interparticle meso- and macropores (0.003 to 1 ?m) within the geopolymer lamellae were only slightly modified by the maturation treatment.

Insights into the macroporosity of freeze-cast hierarchical geopolymers

Papa E;Medri V;Vaccari A;Landi E
2016

Abstract

Geopolymer monoliths with controlled lamellar macroporosity and total porosity ranging from 60% to 70% were prepared by ice-templating a partially geopolymerized slurry. Both the maturation treatment of the starting mixture and the water specifically added for freeze-casting were tailored to modify both the geopolymerization and viscosity of the slurry, and, consequently, its freezing behavior, in order to optimize the final lamellar architecture. Following a room temperature maturation treatment, a 50% water content added for freezing developed thick lamellae and wide pores. A lower water content (30%) and curing at 80 °C after maturation at room temperature (for both 50% and 30% H2O) was conducive to a narrow lamellar pore width distribution in the 30-130 ?m range. However, the consumption of water due to geopolymerization in samples cured at 80 °C led to a decreased length and thickness of the lamellae. Lastly, the interparticle meso- and macropores (0.003 to 1 ?m) within the geopolymer lamellae were only slightly modified by the maturation treatment.
2016
Istituto di Scienza, Tecnologia e Sostenibilità per lo Sviluppo dei Materiali Ceramici - ISSMC (ex ISTEC)
geopolymers; freeze casting
File in questo prodotto:
Non ci sono file associati a questo prodotto.

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/20.500.14243/316686
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus 29
  • ???jsp.display-item.citation.isi??? ND
social impact