Physical aging in high free-volume polymer membranes is one of the main hurdles limiting their ap-plication in gas separation. The recovery of membrane separation properties without the need to dis-assemble the module, although challenging, would provide significant advantages for applications in various fields. In this work, an in situ restoring procedure for the recovery of mass transport in aged membrane modules made of thermally rearranged polymer membranes was developed in which the modules were exposed to methanol at 80 °C. The thermally rearranged hollow fiber membrane modules were subjected to long-time operation to investigate their aging: the CO2 and N2 permeances were monitored at different temperatures, pressures, and feed compositions over a total period of 727 days with two long-time runs of 185 and 263 days, interspersed by a stand-by period of 240 days, and with each run followed by a restoring. In both long-time runs, CO2 and N2 permeance dropped as a result of aging, whereas the selectivity remained nearly constant. The permeances were fully recovered after the proposed restoring procedure was applied, demonstrating its efficacy and repeatability for membrane aging recovery, even for an extremely aged membrane exposed to various conditions for nearly two years.

In situ restoring of aged thermally rearranged gas separation membranes

Brunetti A;Cersosimo M;Drioli E;Barbieri G
2016

Abstract

Physical aging in high free-volume polymer membranes is one of the main hurdles limiting their ap-plication in gas separation. The recovery of membrane separation properties without the need to dis-assemble the module, although challenging, would provide significant advantages for applications in various fields. In this work, an in situ restoring procedure for the recovery of mass transport in aged membrane modules made of thermally rearranged polymer membranes was developed in which the modules were exposed to methanol at 80 °C. The thermally rearranged hollow fiber membrane modules were subjected to long-time operation to investigate their aging: the CO2 and N2 permeances were monitored at different temperatures, pressures, and feed compositions over a total period of 727 days with two long-time runs of 185 and 263 days, interspersed by a stand-by period of 240 days, and with each run followed by a restoring. In both long-time runs, CO2 and N2 permeance dropped as a result of aging, whereas the selectivity remained nearly constant. The permeances were fully recovered after the proposed restoring procedure was applied, demonstrating its efficacy and repeatability for membrane aging recovery, even for an extremely aged membrane exposed to various conditions for nearly two years.
2016
Istituto per la Tecnologia delle Membrane - ITM
Thermally rearranged polymer membrane
aging
restoring
File in questo prodotto:
Non ci sono file associati a questo prodotto.

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/20.500.14243/325615
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus 24
  • ???jsp.display-item.citation.isi??? 22
social impact