Insights about the failure mechanism of negative electrodes based on NaAlH4 for lithium batteries are here discussed based on electrochemical-pressure measurements, galvanostatic cycling, infrared spectroscopy and impedance spectroscopy. The accumulation of irreversible capacity in the first cycle and the capacity fading have multiple origins. Besides the mechanical instability due to volume expansions/contractions upon lithium incorporation/de-incorporation, two additional reasons for electrode failure have been disclosed, both related to active material consumption: (1) the irreversible oxidation upon charge of the alanates that leads to H2 release, and (2) the spontaneous chemical reaction of the electrode active material with the electrolyte due to an unstable solid electrolyte interface. Both problems can be tackled by limiting the anodic voltage cutoffs in lithium cells and by the use of innovative electrolytes based on mixture of an ionic liquid and the standard carbonate-based solvent blend. The use of both strategies allowed us to assemble and demonstrate for few cycles the operation of a full Li-ion cell with a negative electrode based on NaAlH4 and a LiFePO4 positive electrode.

Failure mechanism of NaAlH4 negative electrodes in lithium cells

Brutti S;
2017

Abstract

Insights about the failure mechanism of negative electrodes based on NaAlH4 for lithium batteries are here discussed based on electrochemical-pressure measurements, galvanostatic cycling, infrared spectroscopy and impedance spectroscopy. The accumulation of irreversible capacity in the first cycle and the capacity fading have multiple origins. Besides the mechanical instability due to volume expansions/contractions upon lithium incorporation/de-incorporation, two additional reasons for electrode failure have been disclosed, both related to active material consumption: (1) the irreversible oxidation upon charge of the alanates that leads to H2 release, and (2) the spontaneous chemical reaction of the electrode active material with the electrolyte due to an unstable solid electrolyte interface. Both problems can be tackled by limiting the anodic voltage cutoffs in lithium cells and by the use of innovative electrolytes based on mixture of an ionic liquid and the standard carbonate-based solvent blend. The use of both strategies allowed us to assemble and demonstrate for few cycles the operation of a full Li-ion cell with a negative electrode based on NaAlH4 and a LiFePO4 positive electrode.
2017
Istituto dei Sistemi Complessi - ISC
anodes
failure mechanism
gas release
li-ion batteries
lithium
NaAlH4
negative electrodes
Sodium alanates
File in questo prodotto:
File Dimensione Formato  
prod_377726-doc_127657.pdf

solo utenti autorizzati

Descrizione: Failure mechanism of NaAlH4 negative electrodes in lithium cells
Tipologia: Versione Editoriale (PDF)
Licenza: NON PUBBLICO - Accesso privato/ristretto
Dimensione 2.29 MB
Formato Adobe PDF
2.29 MB Adobe PDF   Visualizza/Apri   Richiedi una copia

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/20.500.14243/332060
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus 10
  • ???jsp.display-item.citation.isi??? 10
social impact