In this work, solutions containing lanthanum salts were used for a post-Treatment of sealing to increase the corrosion resistance of PEO coated AZ91 alloy. PEO coatings were produced on samples of AZ91 magnesium alloy using an alkaline solution containing sodiumhydroxide, sodiumphosphates, and sodiumsilicates.The sealing treatmentwas performed in a solution containing 12 g/L of La(NO3)3 at pH 4 at different temperatures and for different treatment times. Potentiodynamic polarization test, an EIS test, showed that the sealing treatment with solution containing lanthanum nitrate caused a remarkable increase in the corrosion resistance. The corrosion behavior was correlated with the surface morphology and elemental composition evaluated with scanning electron microscope (SEM), X-ray diffraction (XRD), and X-ray photoelectron spectroscopy (XPS). In particular, the sealing treatment at 50°C for 30 min resulted in being the most promising to increase the corrosion properties of PEO treated samples because of the formation of a homogeneous sealing layer, mainly composed of La(OH)3.

Sealing of PEO coated AZ91 magnesium alloy using la-based solutions

Dolcet P;
2017

Abstract

In this work, solutions containing lanthanum salts were used for a post-Treatment of sealing to increase the corrosion resistance of PEO coated AZ91 alloy. PEO coatings were produced on samples of AZ91 magnesium alloy using an alkaline solution containing sodiumhydroxide, sodiumphosphates, and sodiumsilicates.The sealing treatmentwas performed in a solution containing 12 g/L of La(NO3)3 at pH 4 at different temperatures and for different treatment times. Potentiodynamic polarization test, an EIS test, showed that the sealing treatment with solution containing lanthanum nitrate caused a remarkable increase in the corrosion resistance. The corrosion behavior was correlated with the surface morphology and elemental composition evaluated with scanning electron microscope (SEM), X-ray diffraction (XRD), and X-ray photoelectron spectroscopy (XPS). In particular, the sealing treatment at 50°C for 30 min resulted in being the most promising to increase the corrosion properties of PEO treated samples because of the formation of a homogeneous sealing layer, mainly composed of La(OH)3.
2017
Istituto di Chimica della Materia Condensata e di Tecnologie per l'Energia - ICMATE
PLASMA ELECTROLYTIC OXIDATION
CORROSION-RESISTANCE
MG ALLOY
COATINGS
XPS
PHOSPHATE
SILICATE
File in questo prodotto:
Non ci sono file associati a questo prodotto.

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/20.500.14243/341759
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus 33
  • ???jsp.display-item.citation.isi??? ND
social impact