Heterogenization of (eta-Bu4N)(4)W10O32 on amorphous and MCM-41 silicas by impregnation is a suitable method to prepare efficient and stable catalysts able to oxidize unactivated C-H bonds to the corresponding alcohols and ketones with molecular oxygen and near ultraviolet light. The thus-prepared catalysts were characterized by spectroscopic and N-2 adsorption-desorption experiments. A better dispersion of decatungstate was achieved with MCM-41, which also has the higher surface area. Results obtained in the model photooxidation of cyclohexane and cyclododecane confirm that the decatungstate heterogenized on the more ordered MCM-41 silica promotes the process with higher chemoselectivity (cyclohexanone/cyclohexanol molar ratio = 2.6). The photocatalytic efficiency of (n-Bu4N)(4)W10O32 is not reduced after heterogenization; moreover, decatungstate immobilized on amorphous silica oxidizes cyclododecane with a markedly higher efficiency than in the homogeneous phase. The supported photocatalysts can be used at least three times without any loss of activity.

Immobilization of (nbu4n)4W10O32 on mesoporous MCM-41 and amorphous silicas for photocatalytic oxidation of cycloalkanes with molecular oxygen

2002

Abstract

Heterogenization of (eta-Bu4N)(4)W10O32 on amorphous and MCM-41 silicas by impregnation is a suitable method to prepare efficient and stable catalysts able to oxidize unactivated C-H bonds to the corresponding alcohols and ketones with molecular oxygen and near ultraviolet light. The thus-prepared catalysts were characterized by spectroscopic and N-2 adsorption-desorption experiments. A better dispersion of decatungstate was achieved with MCM-41, which also has the higher surface area. Results obtained in the model photooxidation of cyclohexane and cyclododecane confirm that the decatungstate heterogenized on the more ordered MCM-41 silica promotes the process with higher chemoselectivity (cyclohexanone/cyclohexanol molar ratio = 2.6). The photocatalytic efficiency of (n-Bu4N)(4)W10O32 is not reduced after heterogenization; moreover, decatungstate immobilized on amorphous silica oxidizes cyclododecane with a markedly higher efficiency than in the homogeneous phase. The supported photocatalysts can be used at least three times without any loss of activity.
2002
Istituto per la Sintesi Organica e la Fotoreattivita' - ISOF
File in questo prodotto:
Non ci sono file associati a questo prodotto.

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/20.500.14243/36150
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus ND
  • ???jsp.display-item.citation.isi??? ND
social impact