Aromatic polyethersulfone is one of the most used polymeric material for many technological applications. This material possesses a high hydrophobicity, which leads to biofouling phenomena. In order to prepare materials with an optimal balance of hydrophobic and hydrophilic character, a series of aromatic polyethersulfones containing different percentages of 4,4-Bis(4-hydroxyphenyl) pentanoic acid (DPA) units in the main chains was synthesized1. The structure of these polymers show a random distribution of DPA units along the chains, according to a statistical Bernullian theoretical model. Thermal analysis (DSC) shows that the Tg values of copolymers decrease as the amount of DPA units increase. The thermal degradation of the copolymers occurs at a lower temperature with respect to pure PES2,3 due to the presence of DPA units which decompose by losing CO2. For recovering heavy metals from water medium, membranes of PES-DPA copolymers were prepared by electrospinning from DMF solution (Fig.1). Metals (lead, chromium, zinc, cadmium, copper) were recovered by dipping the membrane in aqueous solutions with a concentration of 50ppm, for each metal, and the solution was analysed by ICP-MS. The results show that membranes are able to recovery up to 85% of lead already after 5 minutes of dipping.

SYNTHESIS AND CHARACTERIZATION OF PES COPOLYMERS WITH CARBOXYL UNITS AS METAL RECOVERING MATERIALS

Andrea A Scamporrino;Filippo Samperi;Daniela Zampino;Sandro Dattilo;E Mirabella;Angela Spina;Concetto Puglisi
2019

Abstract

Aromatic polyethersulfone is one of the most used polymeric material for many technological applications. This material possesses a high hydrophobicity, which leads to biofouling phenomena. In order to prepare materials with an optimal balance of hydrophobic and hydrophilic character, a series of aromatic polyethersulfones containing different percentages of 4,4-Bis(4-hydroxyphenyl) pentanoic acid (DPA) units in the main chains was synthesized1. The structure of these polymers show a random distribution of DPA units along the chains, according to a statistical Bernullian theoretical model. Thermal analysis (DSC) shows that the Tg values of copolymers decrease as the amount of DPA units increase. The thermal degradation of the copolymers occurs at a lower temperature with respect to pure PES2,3 due to the presence of DPA units which decompose by losing CO2. For recovering heavy metals from water medium, membranes of PES-DPA copolymers were prepared by electrospinning from DMF solution (Fig.1). Metals (lead, chromium, zinc, cadmium, copper) were recovered by dipping the membrane in aqueous solutions with a concentration of 50ppm, for each metal, and the solution was analysed by ICP-MS. The results show that membranes are able to recovery up to 85% of lead already after 5 minutes of dipping.
2019
Istituto per i Polimeri, Compositi e Biomateriali - IPCB
Inglese
The Fiftieth Anniversary of the Institute for Polymers Composites and Biomaterials
87
87
1
9788880803652
Sì, ma tipo non specificato
metal recovery
PES
polyelectrolites
7
02 Contributo in Volume::02.01 Contributo in volume (Capitolo o Saggio)
268
none
A Scamporrino, Andrea; Samperi, Filippo; Zampino, Daniela; Dattilo, Sandro; Mirabella, E; Spina, Angela; Puglisi, Concetto
info:eu-repo/semantics/bookPart
File in questo prodotto:
Non ci sono file associati a questo prodotto.

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/20.500.14243/367691
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus ND
  • ???jsp.display-item.citation.isi??? ND
social impact