A sample of mesoporous TiO2 (MT, specific surface area = 150 m2g?1) and two samples of MT containing 2.5 wt.% Fe were prepared by either direct synthesis doping (Fe2.5-MTd) or impregnation (Fe2.5-MTi). Commercial TiO2 (Degussa P25, specific surface area = 56 m2g?1) was used both as a benchmark and as a support for impregnation with either 0.8 or 2.5 wt.% Fe (Fe0.80-IT and Fe2.5-IT). The powders were characterized by X-ray diffraction, N2 isotherms at ?196 C, Energy Dispersive X-ray (EDX) Spectroscopy, X-ray Photoelectron Spectroscopy (XPS), Diffuse Reflectance (DR) ultra-violet (UV)-Vis and Mössbauer spectroscopies. Degradation of Acid Orange 7 (AO7) by H2O2 was the test reaction: effects of dark-conditions versus both UV and simulated solar light irradiation were considered. In dark conditions, AO7 conversion was higher with MT than with Degussa P25, whereas Fe-containing samples were active in a (slow) Fenton-like reaction. Under UV light, MT was as active as Degussa P25, and Fe doping enhanced the photocatalytic activity of Fe2.5-MTd; Fe-impregnated samples were also active, likely due to the occurrence of a photo-Fenton process. Interestingly, the Fe2.5-MTd sample showed the best performance under solar light, confirming the positive effect of Fe doping by direct synthesis with respect to impregnation.

Both pure and Fe doped mesoporous titania catalyse the oxidation of Acid Orange 7 by H2O2 in different experimental conditions

2017

Abstract

A sample of mesoporous TiO2 (MT, specific surface area = 150 m2g?1) and two samples of MT containing 2.5 wt.% Fe were prepared by either direct synthesis doping (Fe2.5-MTd) or impregnation (Fe2.5-MTi). Commercial TiO2 (Degussa P25, specific surface area = 56 m2g?1) was used both as a benchmark and as a support for impregnation with either 0.8 or 2.5 wt.% Fe (Fe0.80-IT and Fe2.5-IT). The powders were characterized by X-ray diffraction, N2 isotherms at ?196 C, Energy Dispersive X-ray (EDX) Spectroscopy, X-ray Photoelectron Spectroscopy (XPS), Diffuse Reflectance (DR) ultra-violet (UV)-Vis and Mössbauer spectroscopies. Degradation of Acid Orange 7 (AO7) by H2O2 was the test reaction: effects of dark-conditions versus both UV and simulated solar light irradiation were considered. In dark conditions, AO7 conversion was higher with MT than with Degussa P25, whereas Fe-containing samples were active in a (slow) Fenton-like reaction. Under UV light, MT was as active as Degussa P25, and Fe doping enhanced the photocatalytic activity of Fe2.5-MTd; Fe-impregnated samples were also active, likely due to the occurrence of a photo-Fenton process. Interestingly, the Fe2.5-MTd sample showed the best performance under solar light, confirming the positive effect of Fe doping by direct synthesis with respect to impregnation.
2017
Istituto di Scienze e Tecnologie Molecolari - ISTM - Sede Milano
Inglese
7
213
Sì, ma tipo non specificato
mesoporous titania
soft-template synthesis
azo dyes
iron doping
Fenton reaction
photo-Fenton reaction
photocatalysis
solar light
0
info:eu-repo/semantics/article
262
Francesca S. Freyria; Matteo Compagnoni; Nicoletta Ditaranto; Ilenia Rossetti; Marco Piumetti; Gianguido Ramis;Barbara Bonelli.
01 Contributo su Rivista::01.01 Articolo in rivista
none
File in questo prodotto:
Non ci sono file associati a questo prodotto.

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/20.500.14243/368970
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus ND
  • ???jsp.display-item.citation.isi??? ND
social impact