Cobalt-doped ZnO thin films with several different percentage of Co from 0 up to 15 at% were synthesized via a cheap, simple and versatile method i.e. ultrasonic spray pyrolysis at atmospheric pressure and a substrate temperature of 350 C. The structure of the asprepared samples was characterized by X-ray diffraction (XRD), Raman spectroscopy and FTIR. The Co-doping effect is revealed by the presence of three additional peaks around 235, 470 and 538 cm1 respect to the Raman spectra of the unsubstituted film. Fourier transform infrared spectroscopy (FTIR) put in evidence the decrease of the bond force constant f with increasing Co-doping. By ultra-violet visible near infrared (UVeViseNIR) spectroscopy on Co-doped samples it was possible to show the presence of additional absorption bands at approximately 570, 620 and 660 nm suggesting that Co2þ ions do not change their oxidation when substituted to zinc and the ZnO lattice does not change its wurtzite structure as well. Finally, all our samples exhibit a paramagnetic behavior without any trace of intrinsic room temperature ferromagnetism.

Structural and magnetic properties of Co-doped ZnO thin films grown by ultrasonic spray pyrolysis method

Lamura G;
2017

Abstract

Cobalt-doped ZnO thin films with several different percentage of Co from 0 up to 15 at% were synthesized via a cheap, simple and versatile method i.e. ultrasonic spray pyrolysis at atmospheric pressure and a substrate temperature of 350 C. The structure of the asprepared samples was characterized by X-ray diffraction (XRD), Raman spectroscopy and FTIR. The Co-doping effect is revealed by the presence of three additional peaks around 235, 470 and 538 cm1 respect to the Raman spectra of the unsubstituted film. Fourier transform infrared spectroscopy (FTIR) put in evidence the decrease of the bond force constant f with increasing Co-doping. By ultra-violet visible near infrared (UVeViseNIR) spectroscopy on Co-doped samples it was possible to show the presence of additional absorption bands at approximately 570, 620 and 660 nm suggesting that Co2þ ions do not change their oxidation when substituted to zinc and the ZnO lattice does not change its wurtzite structure as well. Finally, all our samples exhibit a paramagnetic behavior without any trace of intrinsic room temperature ferromagnetism.
2017
Istituto Superconduttori, materiali innovativi e dispositivi - SPIN
Bond force constant
Cobalt doped ZnO
Magnetic properties
Nanostructured thin films
Raman spectroscopy
Ultrasonic spray pyrolysis
Zn[sbnd
File in questo prodotto:
Non ci sono file associati a questo prodotto.

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/20.500.14243/370706
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus 33
  • ???jsp.display-item.citation.isi??? ND
social impact