Silicon-boron alloys have been recently pointed out as novel ultra-high temperature phase change materials for applications in Latent Heat Thermal Energy Storage (LHTES) and conversion systems. One of the emerging challenges related to the development of such devices is a selection of refractories applicable to build a vessel for storing molten Si-B alloys at high temperatures and under consecutive melting/solidification conditions. Previously, it has been documented that hexagonal boron nitride (h-BN) is the only one ceramic showing a non-wettability and limited reactivity with Si-B alloys at temperatures up to 1750 °C, what makes it a good candidate of the first selection for the predicted application. Nevertheless, pure h-BN shows a rather low mechanical strength that could affect a durability of the LHTES vessel. Therefore, the main purpose of this work was to examine high temperature behavior of commercial high strength h-BN composite having a nominal composition of h-BN-24ZrO2-6SiC (vol.%) in contact with a solid/liquid eutectic Si-3.2B alloy. Two types of sessile drop experiments were carried out: a step-contact heating up to 1750 °C, and a thermocycling at 1300 - 1450 °C composed of 15 cycles of the alloy melting/solidification. The obtained results showed a lack of wettability in the examined system at temperatures up to 1750 °C. The Si-3.2B alloy presented good repeatability of melting/solidification temperatures in consecutive thermal cycles, which was not affected by the interaction with the h-BN composite. However, due to reactions taking place between the composite's components leading to structural degradation, it is not recommended to increase operational temperature of this material above 1450 °C.

Silicon-Boron Alloys as New Ultra-High Temperature Phase-Change Materials: Solid/Liquid State Interaction with the h-BN Composite

Giuranno D
2020

Abstract

Silicon-boron alloys have been recently pointed out as novel ultra-high temperature phase change materials for applications in Latent Heat Thermal Energy Storage (LHTES) and conversion systems. One of the emerging challenges related to the development of such devices is a selection of refractories applicable to build a vessel for storing molten Si-B alloys at high temperatures and under consecutive melting/solidification conditions. Previously, it has been documented that hexagonal boron nitride (h-BN) is the only one ceramic showing a non-wettability and limited reactivity with Si-B alloys at temperatures up to 1750 °C, what makes it a good candidate of the first selection for the predicted application. Nevertheless, pure h-BN shows a rather low mechanical strength that could affect a durability of the LHTES vessel. Therefore, the main purpose of this work was to examine high temperature behavior of commercial high strength h-BN composite having a nominal composition of h-BN-24ZrO2-6SiC (vol.%) in contact with a solid/liquid eutectic Si-3.2B alloy. Two types of sessile drop experiments were carried out: a step-contact heating up to 1750 °C, and a thermocycling at 1300 - 1450 °C composed of 15 cycles of the alloy melting/solidification. The obtained results showed a lack of wettability in the examined system at temperatures up to 1750 °C. The Si-3.2B alloy presented good repeatability of melting/solidification temperatures in consecutive thermal cycles, which was not affected by the interaction with the h-BN composite. However, due to reactions taking place between the composite's components leading to structural degradation, it is not recommended to increase operational temperature of this material above 1450 °C.
2020
Istituto di Chimica della Materia Condensata e di Tecnologie per l'Energia - ICMATE
AMADEUS project
Hexagonal boron nitride
Latent heat thermal energy storage
Sessile drop method
Silicon-boron alloys
File in questo prodotto:
Non ci sono file associati a questo prodotto.

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/20.500.14243/383212
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus 4
  • ???jsp.display-item.citation.isi??? ND
social impact