New hydroxyapatite (HAp) ceramics substituted with 10, 30 and 50 at.% of bismuth were synthesized by conventional solid state reaction at high temperature T = 1300 °C, and characterized via X-ray diffraction, scanning electron microscopy, Fourier transform infrared and Raman spectroscopies; dielectric properties were also investigated. The hydroxyl groups observed in infrared spectra confirmed the HAp phase in the studied samples. The crystallite size was estimated by Scherrer's formula and the Williamson-Hall plot, while lattice parameters and the unit cell volume of the samples were measured according to Bi content.Scanning electron microscope images revealed the presence of grains with irregular sizes developed within larger aggregations. Measured relative dielectric permittivity and dielectric loss are slightly affected by Bi content, while the alternating current conductivity increases with a rise frequency, and decreases at increasing of Bi content. The HAp[sbnd]Bi50% sample presents the optimal dielectric properties.

Bismuth-substituted hydroxyapatite ceramics synthesis: Morphological, structural, vibrational and dielectric properties

Capitelli F
2019

Abstract

New hydroxyapatite (HAp) ceramics substituted with 10, 30 and 50 at.% of bismuth were synthesized by conventional solid state reaction at high temperature T = 1300 °C, and characterized via X-ray diffraction, scanning electron microscopy, Fourier transform infrared and Raman spectroscopies; dielectric properties were also investigated. The hydroxyl groups observed in infrared spectra confirmed the HAp phase in the studied samples. The crystallite size was estimated by Scherrer's formula and the Williamson-Hall plot, while lattice parameters and the unit cell volume of the samples were measured according to Bi content.Scanning electron microscope images revealed the presence of grains with irregular sizes developed within larger aggregations. Measured relative dielectric permittivity and dielectric loss are slightly affected by Bi content, while the alternating current conductivity increases with a rise frequency, and decreases at increasing of Bi content. The HAp[sbnd]Bi50% sample presents the optimal dielectric properties.
2019
Vibrational and dielectrical properties
Hydroxyapatite Bismuth Solid State Reaction Microstructure
File in questo prodotto:
Non ci sono file associati a questo prodotto.

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/20.500.14243/408498
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus 18
  • ???jsp.display-item.citation.isi??? ND
social impact