The influence of Y2O3 addition on the microstructure, thermo-mechanical properties and oxidation resistance of carbon fibre reinforced ZrB2/SiC composites was investigated. Y2O3 reacted with oxide impurities present on the surface of ZrB2 and SiC grains and formed a liquid phase, effectively lowering the sintering temperature and allowing to reach full density at 1900 degrees C. The presence of a carbon source (fibres) led to additional reactions which resulted in the formation of new secondary phases such as yttrium boro-carbides. Mechanical properties were significantly enhanced compared to the un-doped composite. Further tests at high temperatures resulted in strength increase up to 700 MPa at 1500 degrees C which was attributed to stress relaxation. Oxidation tests carried out at 1500 degrees C and 1650 degrees C in air showed that the presence of the Y-based secondary phases enhanced the growth of ZrO2 grains, but offered limited protection to oxygen due to the lower availability of surficial SiO2 formed from SiC.

Influence of Y2O3 addition on the mechanical and oxidation behaviour of carbon fibre reinforced ZrB2/SiC composites

Vinci Antonio
Primo
Writing – Original Draft Preparation
;
Zoli Luca
Secondo
Methodology
;
Galizia Pietro
Penultimo
Writing – Review & Editing
;
Sciti Diletta
Ultimo
Funding Acquisition
2020

Abstract

The influence of Y2O3 addition on the microstructure, thermo-mechanical properties and oxidation resistance of carbon fibre reinforced ZrB2/SiC composites was investigated. Y2O3 reacted with oxide impurities present on the surface of ZrB2 and SiC grains and formed a liquid phase, effectively lowering the sintering temperature and allowing to reach full density at 1900 degrees C. The presence of a carbon source (fibres) led to additional reactions which resulted in the formation of new secondary phases such as yttrium boro-carbides. Mechanical properties were significantly enhanced compared to the un-doped composite. Further tests at high temperatures resulted in strength increase up to 700 MPa at 1500 degrees C which was attributed to stress relaxation. Oxidation tests carried out at 1500 degrees C and 1650 degrees C in air showed that the presence of the Y-based secondary phases enhanced the growth of ZrO2 grains, but offered limited protection to oxygen due to the lower availability of surficial SiO2 formed from SiC.
2020
Istituto di Scienza, Tecnologia e Sostenibilità per lo Sviluppo dei Materiali Ceramici - ISSMC (ex ISTEC)
Ceramic-Matrix Composites (CMCs)
Ultra-High-Temperature-Ceramics (UHTCs)
Fibre-matrix interface
Rare earths
Oxidation resistance
File in questo prodotto:
File Dimensione Formato  
Manuscript Y2O3 v2.0 pp.pdf

accesso aperto

Descrizione: postprint
Tipologia: Documento in Post-print
Licenza: Creative commons
Dimensione 1.56 MB
Formato Adobe PDF
1.56 MB Adobe PDF Visualizza/Apri

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/20.500.14243/428312
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus 44
  • ???jsp.display-item.citation.isi??? 38
social impact