The application of titanium dioxide (TiO2) in the photovoltaic (PV) field is gaining traction as this material can be deployed in doping-free heterojunction solar cells with the role of electron selective contact. For modeling-based optimization of such contact, knowledge of the titanium oxide defect density of states (DOS) is crucial. In this paper, we report a method to extract the defect density through nondestructive optical measures, including the contribution given by small polaron optical transitions. The presence of both related to oxygen-vacancy defects and polarons is supported by the results of optical characterizations and the evaluation of previous observations resulting in a defect band fixed at 1 eV below the conduction band edge of the oxide. Solar cells employing pulsed laser deposited-TiO2 electron selective contacts were fabricated and characterized. The J-V curve of these cells showed, however, an S-shape, then a detailed analysis of the reasons for such behavior was carried out. We use a model involving the series of a standard cell equivalent circuit with a Schottky junction in order to explain these atypical performances. A good matching between the experimental measurements and the adopted theoretical model was obtained. The extracted parameters are listed and analyzed to shed light on the reasons behind the low-performance cells.

Density of states characterization of TiO2 films deposited by pulsed laser deposition for heterojunction solar cells

Casaletto Maria Pia;
2021

Abstract

The application of titanium dioxide (TiO2) in the photovoltaic (PV) field is gaining traction as this material can be deployed in doping-free heterojunction solar cells with the role of electron selective contact. For modeling-based optimization of such contact, knowledge of the titanium oxide defect density of states (DOS) is crucial. In this paper, we report a method to extract the defect density through nondestructive optical measures, including the contribution given by small polaron optical transitions. The presence of both related to oxygen-vacancy defects and polarons is supported by the results of optical characterizations and the evaluation of previous observations resulting in a defect band fixed at 1 eV below the conduction band edge of the oxide. Solar cells employing pulsed laser deposited-TiO2 electron selective contacts were fabricated and characterized. The J-V curve of these cells showed, however, an S-shape, then a detailed analysis of the reasons for such behavior was carried out. We use a model involving the series of a standard cell equivalent circuit with a Schottky junction in order to explain these atypical performances. A good matching between the experimental measurements and the adopted theoretical model was obtained. The extracted parameters are listed and analyzed to shed light on the reasons behind the low-performance cells.
2021
solar cell
heterojunction
photovoltaic (PV)
defect density
small polaron
pulsed laser deposition (PLD)
titanium dioxide (TiO2)
defects
File in questo prodotto:
Non ci sono file associati a questo prodotto.

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/20.500.14243/440146
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus ND
  • ???jsp.display-item.citation.isi??? ND
social impact