A synthetic saponite clay containing structural Nb(V) metal centres (NbSAP) was investigated in the abatement of paraoxon-ethyl, an anti-cholinergic organophosphorus pesticide, under mild conditions (neutral pH, room temperature and ambient pressure) in heterogenous phase, without additional basic additives. The material was selected according to its high surface acidity and ease of preparation through a one-step hydrothermal synthesis. The presence of Nb(V) ions played a crucial role in efficiently catalysing the degradation of aggressive chemical substrates. A niobium (V) oxide with very low surface acidity was also tested as a reference material. The study employed a multi-technique approach to monitor the pesticide degradation pathway and byproducts formed during abatement experiments in polar non-protic and aqueous solvents. Notably, in water, the concentration of paraoxon-ethyl significantly decreased by 82 % within the first hour of contact with the clay. Additionally, NbSAP demonstrated a good performance after three repeated catalytic cycles and subsequent reactivation.

Nb(V)-containing saponite: A versatile clay for the catalytic degradation of the hazardous organophosphorus pesticide paraoxon under very mild conditions

Econdi, Stefano
Secondo
;
Guidotti, Matteo
;
2024

Abstract

A synthetic saponite clay containing structural Nb(V) metal centres (NbSAP) was investigated in the abatement of paraoxon-ethyl, an anti-cholinergic organophosphorus pesticide, under mild conditions (neutral pH, room temperature and ambient pressure) in heterogenous phase, without additional basic additives. The material was selected according to its high surface acidity and ease of preparation through a one-step hydrothermal synthesis. The presence of Nb(V) ions played a crucial role in efficiently catalysing the degradation of aggressive chemical substrates. A niobium (V) oxide with very low surface acidity was also tested as a reference material. The study employed a multi-technique approach to monitor the pesticide degradation pathway and byproducts formed during abatement experiments in polar non-protic and aqueous solvents. Notably, in water, the concentration of paraoxon-ethyl significantly decreased by 82 % within the first hour of contact with the clay. Additionally, NbSAP demonstrated a good performance after three repeated catalytic cycles and subsequent reactivation.
2024
Istituto di Scienze e Tecnologie Chimiche "Giulio Natta" - SCITEC - Sede Secondaria Milano - Via C. Golgi
Saponite clay, Paraoxon Pesticide, Catalytic abatement, Environmental remediation, green chemistry
File in questo prodotto:
File Dimensione Formato  
Heliyon-2024-PIIS2405844024159294.pdf

accesso aperto

Descrizione: Heliyon2024
Tipologia: Versione Editoriale (PDF)
Licenza: Creative commons
Dimensione 3.17 MB
Formato Adobe PDF
3.17 MB Adobe PDF Visualizza/Apri
supp info.pdf

accesso aperto

Descrizione: suupplementary information
Tipologia: Altro materiale allegato
Licenza: Altro tipo di licenza
Dimensione 3.15 MB
Formato Adobe PDF
3.15 MB Adobe PDF Visualizza/Apri

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/20.500.14243/511103
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus 1
  • ???jsp.display-item.citation.isi??? ND
social impact