Low-loss hydrogenated amorphous silicon (alpha-Si:H) waveguides were realized by plasma enhanced chemical vapour deposition (PECVD) on a transparent conductive oxide (TCO) layer which is intended to provide the buried contact for the application of an external bias in active devices, e.g. switches and modulators. In particular we propose a technological solution to overcome both the strong reduction in optical transmittance due to the very high extinction coefficient of metal contacts and, at the same time, the optical scattering induced by the texturization effect induced in alpha-Si:H films grown on TCO. The very high optical propagation losses were minimized by depositing a spin-on-glass (SOG) layer between the alpha-Si:H core-layer and the TCO bottom contact. In this case, propagation losses of 2.5 dB/cm at 1550 nm were measured. All the fabricated samples were optically characterized and the surface roughness was accurately measured using a mechanical profilometer. We observed that, for an alpha-Si:H core-layer directly deposited on the TCO contact, the surface roughness is of the order of 100 nm leading to totally opaque waveguides. The experimental performances have been compared to those obtained through calculations using an optical simulation package. The results are found to be in agreement with the experimental data.

Low-loss amorphous silicon waveguides grown by PECVD on indium tin oxide

Summonte C
2010

Abstract

Low-loss hydrogenated amorphous silicon (alpha-Si:H) waveguides were realized by plasma enhanced chemical vapour deposition (PECVD) on a transparent conductive oxide (TCO) layer which is intended to provide the buried contact for the application of an external bias in active devices, e.g. switches and modulators. In particular we propose a technological solution to overcome both the strong reduction in optical transmittance due to the very high extinction coefficient of metal contacts and, at the same time, the optical scattering induced by the texturization effect induced in alpha-Si:H films grown on TCO. The very high optical propagation losses were minimized by depositing a spin-on-glass (SOG) layer between the alpha-Si:H core-layer and the TCO bottom contact. In this case, propagation losses of 2.5 dB/cm at 1550 nm were measured. All the fabricated samples were optically characterized and the surface roughness was accurately measured using a mechanical profilometer. We observed that, for an alpha-Si:H core-layer directly deposited on the TCO contact, the surface roughness is of the order of 100 nm leading to totally opaque waveguides. The experimental performances have been compared to those obtained through calculations using an optical simulation package. The results are found to be in agreement with the experimental data.
2010
Istituto per la Microelettronica e Microsistemi - IMM
amorphous silicon
waveguides
plasma enhanced chemical vapour deposition
transparent conductive oxide
spin on glass
File in questo prodotto:
Non ci sono file associati a questo prodotto.

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/20.500.14243/53662
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus ND
  • ???jsp.display-item.citation.isi??? ND
social impact