ZrO2 and ZrO2-SO3H were used as supports for the preparation of Au-based catalysts for formic acid dehydrogenation. The sulfated zirconium oxide drives the Au dispersion, favouring the formation of small metal nanoparticles and thereby promoting the activity of the resulting catalysts. Two catalyst preparation methods were investigated: incipient-wetness and deposition-precipitation. Deposition-precipitation provides a more finely and uniformly dispersed Au phase than incipient-wetness. The Au/ZrO2-SO3H catalyst prepared by deposition-precipitation reached a remarkable TOF of 1672 h-1 in the presence of triethylamine. A more detailed analysis, involving the calculation of TOFs normalized to surface, high-coordination-number and low-coordination-number Au sites, suggests a major contribution of edge and corner atoms to the catalytic activity. Furthermore, the replacement of triethylamine with non-toxic and accessible amino acids was also evaluated. In particular, glycine and l-arginine proved to be promising substitutes for conventional amines in formic acid dehydrogenation. In the presence of l-arginine, the Au/ZrO2-SO3H prepared by deposition-precipitation achieved a TOF of 865 h-1.

Promoting effect of sulfated zirconia on the activity of Au catalysts for formic acid dehydrogenation mediated by amino acids

Evangelisti, Claudio;Ardemani, Leandro;Scotti, Nicola;Ravasio, Nicoletta;Zaccheria, Federica
2026

Abstract

ZrO2 and ZrO2-SO3H were used as supports for the preparation of Au-based catalysts for formic acid dehydrogenation. The sulfated zirconium oxide drives the Au dispersion, favouring the formation of small metal nanoparticles and thereby promoting the activity of the resulting catalysts. Two catalyst preparation methods were investigated: incipient-wetness and deposition-precipitation. Deposition-precipitation provides a more finely and uniformly dispersed Au phase than incipient-wetness. The Au/ZrO2-SO3H catalyst prepared by deposition-precipitation reached a remarkable TOF of 1672 h-1 in the presence of triethylamine. A more detailed analysis, involving the calculation of TOFs normalized to surface, high-coordination-number and low-coordination-number Au sites, suggests a major contribution of edge and corner atoms to the catalytic activity. Furthermore, the replacement of triethylamine with non-toxic and accessible amino acids was also evaluated. In particular, glycine and l-arginine proved to be promising substitutes for conventional amines in formic acid dehydrogenation. In the presence of l-arginine, the Au/ZrO2-SO3H prepared by deposition-precipitation achieved a TOF of 865 h-1.
2026
Istituto di Scienze e Tecnologie Chimiche "Giulio Natta" - SCITEC - Sede Secondaria Milano - Via C. Golgi
Istituto di Chimica dei Composti Organo Metallici - ICCOM - Sede Secondaria Pisa
ZrO2, ZrO2-SO3H, Au-based catalysts, formic acid dehydrogenation
File in questo prodotto:
File Dimensione Formato  
RSC Adv., 2026, 16, 72084–72093.pdf

accesso aperto

Descrizione: VoR
Tipologia: Versione Editoriale (PDF)
Licenza: Creative commons
Dimensione 862.1 kB
Formato Adobe PDF
862.1 kB Adobe PDF Visualizza/Apri
si_revised_un_marked_suppl.pdf

accesso aperto

Descrizione: supporting information
Tipologia: Versione Editoriale (PDF)
Licenza: Creative commons
Dimensione 1.38 MB
Formato Adobe PDF
1.38 MB Adobe PDF Visualizza/Apri

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/20.500.14243/609208
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus ND
  • ???jsp.display-item.citation.isi??? 0
social impact