The present work focuses on the X-ray Photoelectron Spectroscopy (XPS) and X-ray Excited Auger Electron Spectroscopy (XE-AES) of a Co3O4/ZnO nanosystem. The composite material was obtained via a two-step Plasma Enhanced-Chemical Vapor Deposition (PECVD) process in Ar/O2 mixtures, consisting in the initial deposition of ZnO and the subsequent growth of Co3O4 onto the pristine matrices. Zn(ketoimi)2 (ketoimi = [CH3O(CH2)3NC(CH3)=C(H)C(CH3)=O]) and Co(dpm)2 (dpm = 2,2,6,6-tetramethyl-3,5-heptanedionate) were used as zinc and cobalt precursors, respectively. In particular, strongly <001> oriented ZnO was grown at 300°C, followed by the growth of Co3O4 at 200°C, applying a radio-frequency (RF) power of 20 W. Structural, morphological and compositional investigations were performed by Glancing Incidence X-ray Diffraction (GIXRD), Field Emission-Scanning Electron Microscopy (FE-SEM) and Energy Dispersive X-ray Spectroscopy (EDXS). Surface XPS and XE-AES analyses were carried out to study in detail the O1s, Zn2p3/2, Zn3p and Co2p core levels, as well as the Zn and Co Auger peaks of the composite material. The obtained results evidenced the formation of a composite material, in which ZnO and Co3O4 preserved their chemical identity.

p-Co3O4/n-ZnO, obtained by PECVD, analyzed by X-ray Photoelectron Spectroscopy

BARRECA, DAVIDE
2011

Abstract

The present work focuses on the X-ray Photoelectron Spectroscopy (XPS) and X-ray Excited Auger Electron Spectroscopy (XE-AES) of a Co3O4/ZnO nanosystem. The composite material was obtained via a two-step Plasma Enhanced-Chemical Vapor Deposition (PECVD) process in Ar/O2 mixtures, consisting in the initial deposition of ZnO and the subsequent growth of Co3O4 onto the pristine matrices. Zn(ketoimi)2 (ketoimi = [CH3O(CH2)3NC(CH3)=C(H)C(CH3)=O]) and Co(dpm)2 (dpm = 2,2,6,6-tetramethyl-3,5-heptanedionate) were used as zinc and cobalt precursors, respectively. In particular, strongly <001> oriented ZnO was grown at 300°C, followed by the growth of Co3O4 at 200°C, applying a radio-frequency (RF) power of 20 W. Structural, morphological and compositional investigations were performed by Glancing Incidence X-ray Diffraction (GIXRD), Field Emission-Scanning Electron Microscopy (FE-SEM) and Energy Dispersive X-ray Spectroscopy (EDXS). Surface XPS and XE-AES analyses were carried out to study in detail the O1s, Zn2p3/2, Zn3p and Co2p core levels, as well as the Zn and Co Auger peaks of the composite material. The obtained results evidenced the formation of a composite material, in which ZnO and Co3O4 preserved their chemical identity.
2011
Istituto di Chimica della Materia Condensata e di Tecnologie per l'Energia - ICMATE
Istituto di Scienze e Tecnologie Molecolari - ISTM - Sede Milano
Inglese
18
1
36
45
10
http://scitation.aip.org/content/avs/journal/sss/18/1/10.1116/11.20111003
Sì, ma tipo non specificato
Co3O4/ZnO
Nanocomposite
PECVD
XE-AES
XPS
rivista non-ISI
1
info:eu-repo/semantics/article
262
Barreca, Davide
01 Contributo su Rivista::01.01 Articolo in rivista
none
File in questo prodotto:
Non ci sono file associati a questo prodotto.

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/20.500.14243/116367
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus 8
  • ???jsp.display-item.citation.isi??? 8
social impact