Entropy-stabilized (Hf,Nb,Ta,Ti,Zr)B solid solution powders produced by a carbo/boro-thermal reduction followed by solid solution formation were first analysed by synchrotron radiation x-ray diffraction, and their long range periodicity (i.e. lattice parameters) as well as the micro-strain intended as lattice disorder were quantitatively determined. A model to describe the micro-strain was proposed. The as-synthesized (Hf,Nb,Ta,Ti,Zr)B solid solution powders were then hot-pressed at 2200 K and 50 MPa until near full densification was achieved. The hot-pressed material had a residual micro-porosity of 1.3 vol.% and consisted of a (Hf,Nb,Ta,Ti,Zr)B ceramic matrix, 0.3-1 ?m grain size range, and of a residual 10 vol.% BC particulate component, grain size in the range 0.2-2 ?m. BC was a side product of the former synthesis and, after hot-pressing, remained trapped along the grain boundaries of the primary (Hf,Nb,Ta,Ti,Zr)B solid solution ceramic matrix. Micro-hardness HV = 22.7 ± 1.9 GPa for 1.96 N applied force was measured.

Compositional disorder and sintering of entropy stabilized (Hf,Nb,Ta,Ti,Zr)B2 solid solution powders

Monteverde F
Primo
Writing – Original Draft Preparation
;
Saraga F
Secondo
Membro del Collaboration Group
;
2020

Abstract

Entropy-stabilized (Hf,Nb,Ta,Ti,Zr)B solid solution powders produced by a carbo/boro-thermal reduction followed by solid solution formation were first analysed by synchrotron radiation x-ray diffraction, and their long range periodicity (i.e. lattice parameters) as well as the micro-strain intended as lattice disorder were quantitatively determined. A model to describe the micro-strain was proposed. The as-synthesized (Hf,Nb,Ta,Ti,Zr)B solid solution powders were then hot-pressed at 2200 K and 50 MPa until near full densification was achieved. The hot-pressed material had a residual micro-porosity of 1.3 vol.% and consisted of a (Hf,Nb,Ta,Ti,Zr)B ceramic matrix, 0.3-1 ?m grain size range, and of a residual 10 vol.% BC particulate component, grain size in the range 0.2-2 ?m. BC was a side product of the former synthesis and, after hot-pressing, remained trapped along the grain boundaries of the primary (Hf,Nb,Ta,Ti,Zr)B solid solution ceramic matrix. Micro-hardness HV = 22.7 ± 1.9 GPa for 1.96 N applied force was measured.
2020
Istituto di Scienza, Tecnologia e Sostenibilità per lo Sviluppo dei Materiali Ceramici - ISSMC (ex ISTEC)
ultra-high temperature ceramisc
synchrotron radiation
microstrain
entropy stabilization
solid solution
ceramics
mechanical properties
File in questo prodotto:
File Dimensione Formato  
1-s2.0-S0955221920302946-main.pdf

solo utenti autorizzati

Tipologia: Versione Editoriale (PDF)
Licenza: NON PUBBLICO - Accesso privato/ristretto
Dimensione 4.96 MB
Formato Adobe PDF
4.96 MB Adobe PDF   Visualizza/Apri   Richiedi una copia
FMonteverde et al_Compositional disorder and sintering_1_rev_13032020.pdf

accesso aperto

Tipologia: Documento in Post-print
Licenza: Altro tipo di licenza
Dimensione 1.99 MB
Formato Adobe PDF
1.99 MB Adobe PDF Visualizza/Apri

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/20.500.14243/396418
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus 41
  • ???jsp.display-item.citation.isi??? 37
social impact