This investigation introduces two new techniques to quantitatively address the challenging problem of understanding Hydrogen Induced Cracking (HIC) in welding processes. The first technique is a novel procedure to create a known and controlled HIC in a welded sample. The second is an in-process monitoring technique to measure the initial formation and subsequent growth of the HIC in a multi-pass weld whilst being compatible with the high temperatures associated with the welding process. The HIC was initiated using a localised quenching method of the weld and its character was verified using both macrograph and microscopic investigations. During HIC initiation and growth, the sample was monitored every 1-30 min for a total of 96 h using a custom non-destructive testing (NDT) system, mounted on a robot which ensured repeatable inspection positioning. Combining these techniques has therefore allowed for the first time, a detailed understanding of the evolution of HIC in a multi-pass welded sample. Our findings reveal that the HIC was initiated 43 min after the weld ended and that it then grew rapidly for about 15 min and continued growing at a slower rate for around 24 h. No significant growth was observed for the remaining 72 h of the experimental measurement.

High-temperature in-process inspection followed by 96-h robotic inspection of intentionally manufactured hydrogen crack in multi-pass robotic welding

Mineo Carmelo;
2021

Abstract

This investigation introduces two new techniques to quantitatively address the challenging problem of understanding Hydrogen Induced Cracking (HIC) in welding processes. The first technique is a novel procedure to create a known and controlled HIC in a welded sample. The second is an in-process monitoring technique to measure the initial formation and subsequent growth of the HIC in a multi-pass weld whilst being compatible with the high temperatures associated with the welding process. The HIC was initiated using a localised quenching method of the weld and its character was verified using both macrograph and microscopic investigations. During HIC initiation and growth, the sample was monitored every 1-30 min for a total of 96 h using a custom non-destructive testing (NDT) system, mounted on a robot which ensured repeatable inspection positioning. Combining these techniques has therefore allowed for the first time, a detailed understanding of the evolution of HIC in a multi-pass welded sample. Our findings reveal that the HIC was initiated 43 min after the weld ended and that it then grew rapidly for about 15 min and continued growing at a slower rate for around 24 h. No significant growth was observed for the remaining 72 h of the experimental measurement.
2021
Istituto di Calcolo e Reti ad Alte Prestazioni - ICAR
Crack growth monitoring
Hydrogen induced cracks
Intentionally embedded defects
Phased array ultrasonic testing (PAUT)
Robotic nondestructive testing
Robotic welding
File in questo prodotto:
Non ci sono file associati a questo prodotto.

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/20.500.14243/444223
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus 16
  • ???jsp.display-item.citation.isi??? ND
social impact