The effects of 2 MeV Si+ implantation on silicon-on-insulator layers uniformly doped with B at concentrations 1.0 and 1.81020 cm-3, and the kinetics of damage recovery were investigated by carrier density, mobility measurements, and transmission electron microscopy TEM observations. High energy implantation reduces the hole density by about 98%; the mobility is also reduced at an extent which increases with B concentration. Isochronal and isothermal annealings show that recovery of the hole density takes place in three stages: the first stage is accompanied by a mobility decrease and is followed by the second stage where mobility increases attaining values close to the ones of the reference undamaged samples. Mobility keeps nearly constant in the third recovery stage , which takes place above 800 °C. As a characterizing feature the mobility values for each B concentration only depend on the hole density, irrespective of the thermal history of the samples. Experiments and TEM observations allowed us to distinguish defect recovery from SiB3 precipitation, which can take place at temperatures higher than 700 °C. Recovery stages are discussed, and it is concluded that dissolution of B rich clusters in stage modifies the concentration, or the charge state, of the defects responsible of the second stage. These defects are identified as boron interstitial clusters in consideration of their mobility behavior and of the activation energy E for their recovery process, which results to be 3±0.2 eV.

Damage recovery in boron doped silicon on insulator layers after high energy Si+ implantation

M Ferri;S Solmi;
2006

Abstract

The effects of 2 MeV Si+ implantation on silicon-on-insulator layers uniformly doped with B at concentrations 1.0 and 1.81020 cm-3, and the kinetics of damage recovery were investigated by carrier density, mobility measurements, and transmission electron microscopy TEM observations. High energy implantation reduces the hole density by about 98%; the mobility is also reduced at an extent which increases with B concentration. Isochronal and isothermal annealings show that recovery of the hole density takes place in three stages: the first stage is accompanied by a mobility decrease and is followed by the second stage where mobility increases attaining values close to the ones of the reference undamaged samples. Mobility keeps nearly constant in the third recovery stage , which takes place above 800 °C. As a characterizing feature the mobility values for each B concentration only depend on the hole density, irrespective of the thermal history of the samples. Experiments and TEM observations allowed us to distinguish defect recovery from SiB3 precipitation, which can take place at temperatures higher than 700 °C. Recovery stages are discussed, and it is concluded that dissolution of B rich clusters in stage modifies the concentration, or the charge state, of the defects responsible of the second stage. These defects are identified as boron interstitial clusters in consideration of their mobility behavior and of the activation energy E for their recovery process, which results to be 3±0.2 eV.
2006
Istituto per la Microelettronica e Microsistemi - IMM
File in questo prodotto:
Non ci sono file associati a questo prodotto.

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/20.500.14243/11410
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus ND
  • ???jsp.display-item.citation.isi??? ND
social impact