In this work, a FAA3-50 anion-exchange membrane (from FuMa-Tech) has been used, after exchange in KOH solution (1 M), as electrolyte/separator in a single cell of 5 cm2 geometrical area. In the first approach, commercial IrO2 and 40% Pt/C catalysts have been used at the anode and cathode, respectively, to evaluate the membrane under the most convenient conditions. The influence of cell temperature, membrane-electrode assembly (MEA) procedure (catalyst-coated membrane or catalyst coated electrode), ionomer content in the electrodes, use of pure water or KOH solution, on electrolyser performance have been analysed.

INFLUENCE OF OPERATING CONDITIONS ON THE PERFORMANCE OF AN ANION EXCHANGE MEMBRANE ELECTROLYSER

Baglio V;Lo Vecchio C;Zignani S;Trocino S;Monforte G;Patti A;Gatto I
2022

Abstract

In this work, a FAA3-50 anion-exchange membrane (from FuMa-Tech) has been used, after exchange in KOH solution (1 M), as electrolyte/separator in a single cell of 5 cm2 geometrical area. In the first approach, commercial IrO2 and 40% Pt/C catalysts have been used at the anode and cathode, respectively, to evaluate the membrane under the most convenient conditions. The influence of cell temperature, membrane-electrode assembly (MEA) procedure (catalyst-coated membrane or catalyst coated electrode), ionomer content in the electrodes, use of pure water or KOH solution, on electrolyser performance have been analysed.
2022
Istituto di Tecnologie Avanzate per l'Energia - ITAE
Water electrolysis
File in questo prodotto:
Non ci sono file associati a questo prodotto.

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/20.500.14243/420050
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus ND
  • ???jsp.display-item.citation.isi??? ND
social impact