Metal-oxide-semiconductor (MOS) capacitors with Al2O3 as a gate insulator are fabricated on cubic silicon carbide (3C-SiC). Al2O3 is deposited both by thermal and plasma-enhanced Atomic Layer Deposition (ALD) on a thermally grown 5 nm SiO2 interlayer to improve the ALD nucleation and guarantee a better band offset with the SiC. The deposited Al2O3/SiO2 stacks show lower negative shifts of the flat band voltage VFB (in the range of about −3 V) compared with the conventional single SiO2 layer (in the range of −9 V). This lower negative shift is due to the combined effect of the Al2O3 higher permittivity (ε = 8) and to the reduced amount of carbon defects generated during the short thermal oxidation process for the thin SiO2. Moreover, the comparison between thermal and plasma-enhanced ALD suggests that this latter approach produces Al2O3 layers possessing better insulating behavior in terms of distribution of the leakage current breakdown. In fact, despite both possessing a breakdown voltage of 26 V, the T-ALD Al2O3 sample is characterised by a higher current density starting from 15 V. This can be attributable to the slightly inferior quality (in terms of density and defects) of Al2O3 obtained by the thermal approach and, which also explains its non-uniform dC/dV distribution arising by SCM maps.

Al2O3 Layers Grown by Atomic Layer Deposition as Gate Insulator in 3C-SiC MOS Devices

Schiliro, Emanuela
;
Fiorenza, Patrick;Lo Nigro, Raffaella;Galizia, Bruno;Greco, Giuseppe;Di Franco, Salvatore;Bongiorno, Corrado;La Via, Francesco;Giannazzo, Filippo;Roccaforte, Fabrizio
2023

Abstract

Metal-oxide-semiconductor (MOS) capacitors with Al2O3 as a gate insulator are fabricated on cubic silicon carbide (3C-SiC). Al2O3 is deposited both by thermal and plasma-enhanced Atomic Layer Deposition (ALD) on a thermally grown 5 nm SiO2 interlayer to improve the ALD nucleation and guarantee a better band offset with the SiC. The deposited Al2O3/SiO2 stacks show lower negative shifts of the flat band voltage VFB (in the range of about −3 V) compared with the conventional single SiO2 layer (in the range of −9 V). This lower negative shift is due to the combined effect of the Al2O3 higher permittivity (ε = 8) and to the reduced amount of carbon defects generated during the short thermal oxidation process for the thin SiO2. Moreover, the comparison between thermal and plasma-enhanced ALD suggests that this latter approach produces Al2O3 layers possessing better insulating behavior in terms of distribution of the leakage current breakdown. In fact, despite both possessing a breakdown voltage of 26 V, the T-ALD Al2O3 sample is characterised by a higher current density starting from 15 V. This can be attributable to the slightly inferior quality (in terms of density and defects) of Al2O3 obtained by the thermal approach and, which also explains its non-uniform dC/dV distribution arising by SCM maps.
2023
Istituto per la Microelettronica e Microsistemi - IMM
3C-SiC
ALD
WBG
dielectrics
high-κ
File in questo prodotto:
File Dimensione Formato  
materials2023.pdf

accesso aperto

Tipologia: Versione Editoriale (PDF)
Licenza: Creative commons
Dimensione 2.28 MB
Formato Adobe PDF
2.28 MB Adobe PDF Visualizza/Apri

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/20.500.14243/515051
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus 3
  • ???jsp.display-item.citation.isi??? 3
social impact